Casting standards & grades

A quick reference to the cast grades buyers most often specify, with approximate equivalents across ASTM, EN and wrought designations.

How to read cast-steel designations

ASTM cast stainless and heat-resistant grades follow the Alloy Casting Institute system. The first letter shows the service: C for corrosion-resistant, H for heat-resistant. The second letter indicates the approximate nickel-chromium balance (moving up the alphabet as nickel increases). The number is the maximum carbon in hundredths of a percent, and any trailing letters show extra elements, such as M for molybdenum or N for nitrogen. So CF8M = corrosion-resistant, ~19Cr-10Ni type, 0.08% C max, with molybdenum.

EN grades are given by name (for example GX5CrNiMo19-11-2) and by material number (1.4408). IS grades (for example IS 1030 230-450W) give minimum tensile and yield strengths, with W marking a weldable variant.

We cast to ASTM, DIN, EN, BS, IS and proprietary specifications, up to 180 kg per piece.

Carbon steel

General-purpose and pressure-service grades.

GradeStandardApprox. equivalentTypical use
WCBASTM A216EN 10213 GP240GH (1.0619)Valve bodies, flanges, fittings
WCCASTM A216EN 10213 GP280GH (1.0625)Higher-strength pressure parts
LCB / LCCASTM A352EN 10213 G20Mn5 (1.6220)Low-temperature pressure parts
65-35 / 70-36ASTM A27IS 1030 230-450 / 280-520General engineering castings
230-450W / 280-520WIS 1030ASTM A27 (approx.)Weldable general castings

Alloy steel

Chrome-moly grades for high-temperature pressure service, plus heat-treatable structural grades.

GradeStandardApprox. equivalentTypical use
WC6ASTM A217EN 10213 G17CrMo5-5 (1.7357)High-temperature steam valves
WC9ASTM A217EN 10213 G17CrMo9-10 (1.7379)Higher-temperature pressure parts
C5ASTM A2175Cr-0.5MoRefinery service
C12ASTM A2179Cr-1MoElevated temperature, sulphur-bearing media
SC4130 / SC4140ASTM A958AISI 4130 / 4140 (cast)High-strength machine parts
Grade 4, Class A–DASTM A487Ni-Cr-Mo low alloyHigher-strength pressure parts

Heat-resistant steel (HRCS)

For service above roughly 650 °C.

GradeStandardApprox. equivalentTypical use
HFASTM A29719Cr-9NiModerate-temperature furnace parts
HHASTM A297EN 10295 GX40CrNiSi25-12 (1.4837)Furnace fixtures, grates
HKASTM A297EN 10295 GX40CrNiSi25-20 (1.4848)Radiant and higher-strength furnace parts
HTASTM A29735Ni-15CrThermal-cycling fixtures
HPASTM A29735Ni-25CrPetrochemical high-temperature service

Stainless steel

Austenitic and martensitic corrosion-resistant grades. ASTM A743 covers general corrosion-resistant service; ASTM A744 covers the same grade family for severe service.

GradeStandardApprox. equivalentTypical use
CF8ASTM A351 / A743304 · EN 1.4308Valves, pumps, general corrosion
CF8MASTM A351 / A743316 · EN 1.4408Chlorides, chemical media
CF3 / CF3MASTM A351304L / 316L · EN 1.4309 / 1.4409Welded assemblies
CN7MASTM A351 / A743Alloy 20 typeSulphuric acid service
CA15ASTM A217 / A743410Valve trim, mild corrosion and wear
CA6NMASTM A743 / A48713Cr-4Ni · EN 1.4317Impellers, pump casings, turbines

Duplex & super duplex

A890 covers general service; A995 covers pressure-containing parts.

GradeStandardApprox. equivalentTypical use
1B (CD4MCuN)ASTM A890 / A99525Cr duplex + CuSlurry and abrasive-corrosive pumps
4A (CD3MN)ASTM A890 / A9952205 type · EN 1.4470Valves, pumps, chemical process
5A (CE3MN)ASTM A890 / A9952507 type · EN 1.4469Seawater, offshore, desalination
6A (CD3MWCuN)ASTM A890 / A99525Cr super duplex + W, CuSeawater and firewater systems

Nickel-base alloys

ASTM A494 cast nickel alloys and their wrought counterparts.

GradeStandardApprox. equivalentTypical use
CZ-100ASTM A494Nickel 200Caustic alkalis
M35-1ASTM A494Alloy 400 (Ni-Cu)Seawater, hydrofluoric acid
CY-40ASTM A494Alloy 600 (Ni-Cr-Fe)High-temperature, caustic service
CW-6MCASTM A494Alloy 625Severe chloride and acid service
CW-12MW / CW-2MASTM A494C-276 / C-4 typeMixed acids, wet chlorine
N-12MV / N-7MASTM A494B / B-2 typeHydrochloric acid
CU5MCuCASTM A494Alloy 825 (Incoloy type)Sulphuric and phosphoric acids

High-chrome & Ni-hard iron

Abrasion-resistant white irons to ASTM A532.

GradeStandardApprox. equivalentTypical use
Class I Type A, B, CASTM A532Ni-Cr (Ni-hard)Wear parts in dry abrasion
Class I Type DASTM A532Ni-Cr, higher chromiumSlurry pump parts, liners
Class II Type A, DASTM A532Cr-Mo (high-chrome)Slurry pump parts, mill and chute liners

Manganese steel

Austenitic manganese (Hadfield) steel; work-hardens under impact.

GradeStandardApprox. equivalentTypical use
Grade A, B, C, DASTM A128Hadfield-type, ~11%+ MnTeeth, liners, wear parts under impact

Grey & SG iron

Cast irons for housings, bodies and machine parts.

GradeStandardApprox. equivalentTypical use
Various classes, e.g. Class 30ASTM A48Grey (flake graphite) ironHousings, machine bases
Various grades, e.g. 65-45-12ASTM A536SG / ductile ironValve and pump bodies, housings