In short

Alloy steels add chromium, molybdenum, nickel or other elements to carbon steel for higher strength, hardenability and resistance to high-temperature creep. H.J. MetalCraft is an alloy steel casting manufacturer in India, casting low- and high-alloy steels up to 180 kg, heat-treated in-house to grades such as ASTM A217 WC6 and WC9.

Power plant pipework

What is alloy steel?

Alloy cast steels contain deliberate additions of elements such as chromium, molybdenum, nickel and vanadium. Low-alloy steels (typically under 8% total alloy) gain hardenability and strength after quenching and tempering, while chrome-moly grades resist creep and oxidation at the high temperatures found in steam and process plant. High-alloy steels go further and overlap with stainless and heat-resistant grades.

Commonly specified grades

Grade Standard Composition Typical use
WC6 ASTM A217 1.25Cr-0.5Mo Valves and fittings for high-temperature steam
WC9 ASTM A217 2.25Cr-1Mo Higher-temperature pressure parts
C5 ASTM A217 5Cr-0.5Mo Refinery and hydrogen service
C12 ASTM A217 9Cr-1Mo Elevated temperature, sulphur-bearing media
Grade 4, Class A, B, C, D ASTM A487 Ni-Cr-Mo low alloy, normalised or quenched and tempered by class Higher-strength pressure parts, e.g. oil and gas
SC4130 / SC4140 ASTM A958 Cr-Mo, heat-treatable High-strength machine parts
G17CrMo5-5 (1.7357) EN 10213 1.25Cr-0.5Mo European pressure specifications

Where alloy steel castings are used

  • Power generation: valve bodies and fittings for high-pressure, high-temperature steam
  • Oil and petrochemical: pressure-retaining parts in refinery and process service
  • Automobile and general engineering: gears, couplings, hubs and high-strength structural parts
  • Cement and mining: parts needing strength and toughness under heavy load

Heat treatment makes the grade

The properties of alloy steel depend on heat treatment. Our gas-fired bogie furnace (1.0 t capacity) handles water quenching, normalising and annealing, a second bogie furnace with indirect flame handles tempering, and the 14,000-litre agitated quench tank gives a fast, even quench. Proof stress, tensile strength and hardness are then confirmed on our 200 kN universal testing machine and computerised Brinell tester.

Tips for your enquiry

  1. Give the grade, standard and required heat-treatment condition.
  2. Specify mechanical properties or hardness range if your drawing calls for them.
  3. Note any post-weld heat treatment or weld-repair restrictions.

Frequently asked questions

What is ASTM A217 WC6 used for?

WC6 is a 1.25% chromium, 0.5% molybdenum cast steel used for valves, flanges and fittings in high-temperature steam and process service, where it resists creep better than carbon steel.

Do you heat-treat alloy steel castings in-house?

Yes. We have gas-fired bogie furnaces for quenching, normalising, annealing and tempering, plus a 14,000-litre agitated water quench tank.

How do you confirm the chemistry of alloy steel?

Chemistry is analysed on our PMT and CCD spectrometers, which cover up to 32 elements for ferrous alloys.