Material guide
Manganese steel castings
In short
Austenitic manganese steel, often called Hadfield steel, hardens at the surface when it is hit, while the core stays tough. H.J. MetalCraft is a manganese steel casting manufacturer in India, casting to ASTM A128 Grades A, B, C and D, up to 180 kg per piece, for wear parts that take repeated impact.

What is manganese steel?
Austenitic manganese steel contains roughly 1% carbon and 11% or more manganese. After heat treatment it is tough and fairly soft, but under repeated impact its surface work-hardens sharply while the core stays ductile. That combination makes it the standard material for parts that are struck, crushed or gouged, rather than simply rubbed.
It is non-magnetic in its normal condition and must be water-quenched from a high temperature to keep carbides in solution; slow cooling makes it brittle.
Grades we cast
ASTM A128 covers austenitic manganese steel castings. We cast Grades A, B, C and D, which differ in carbon and manganese content and, for some grades, chromium, nickel or molybdenum additions. Send your grade and drawing and ask us to confirm the grade before ordering.
Where it is used
- Earth-moving and mining: teeth, adaptors, liners and wear plates
- Crushing and quarrying: smaller crusher wear parts and hammers, within our 180 kg limit
- Cement: wear parts that take impact as well as abrasion
Manganese steel only work-hardens if the part is hit hard enough. For sliding or slurry wear without impact, an abrasion-resistant iron such as high-chrome or Ni-hard usually lasts longer.
Heat treatment
Manganese steel castings are solution-treated and then quenched in water. Our gas-fired bogie furnace handles the heating, and the 14,000-litre agitated quench tank gives the fast, even quench these castings need.
Tips for your enquiry
- Give the ASTM A128 grade, or describe the impact and wear the part sees.
- Say whether any faces must be machined: work-hardening makes manganese steel hard to machine, so keep machined features to a minimum.
- Tell us the part weight; heavy crusher parts above 180 kg are outside our range.
Frequently asked questions
Which manganese steel grades do you cast?
ASTM A128 Grades A, B, C and D, up to 180 kg per piece. Send your grade and drawing and we will confirm it.
Why is manganese steel water-quenched?
Quenching from a high temperature keeps carbides dissolved and the structure fully austenitic, which makes the steel tough. Slow cooling lets carbides form at the grain boundaries and makes it brittle.
When should I choose manganese steel over high-chrome iron?
Choose manganese steel where the part takes heavy, repeated impact. For abrasion with little impact, such as slurry or sliding wear, a high-chrome or Ni-hard iron usually lasts longer.