Materials
CF8 vs CF8M vs CF3M: which cast stainless grade?
CF8, CF8M and CF3M are the cast equivalents of 304, 316 and 316L. This guide compares their chemistry and properties and explains when to choose each.
· Husein Jazakallah, Managing Director
CF8, CF8M and CF3M are the cast forms of 304, 316 and 316L stainless steel. Choose CF8 for general corrosion service without chlorides. Choose CF8M when chlorides or pitting are a concern, because it contains 2–3% molybdenum. Choose CF3M when the casting will be welded and not re-annealed, because its carbon is held to 0.03%.
How do CF8, CF8M and CF3M compare?
All three are austenitic chromium-nickel grades in ASTM A351, the specification for austenitic castings for pressure-containing parts. The differences that matter most are molybdenum and carbon. Their minimum strengths are the same.
| CF8 | CF8M | CF3M | |
|---|---|---|---|
| Carbon, max (%) | 0.08 | 0.08 | 0.03 |
| Chromium (%) | 18.0–21.0 | 18.0–21.0 | 17.0–21.0 |
| Nickel (%) | 8.0–11.0 | 9.0–12.0 | 9.0–13.0 |
| Molybdenum (%) | 0.50 max | 2.0–3.0 | 2.0–3.0 |
| Tensile strength, min | 485 MPa (70 ksi) | 485 MPa (70 ksi) | 485 MPa (70 ksi) |
| Yield strength, min | 205 MPa (30 ksi) | 205 MPa (30 ksi) | 205 MPa (30 ksi) |
| Elongation, min | 35% | 30% | 30% |
| Nearest wrought grade | 304 | 316 | 316L |
| Nearest EN cast grade | 1.4308 | 1.4408 | 1.4409 |
| UNS | J92600 | J92900 | J92800 |
Chemistry and properties are per ASTM A351, in the solution-annealed condition. All three grades are solution annealed at 1040°C (1900°F) minimum and quenched in water or cooled rapidly, as described in our heat treatment guide.
The cast grades are not exact copies of the wrought ones. Their chromium and nickel ranges are set so that the castings contain some ferrite, which helps resist hot cracking. The EN grades in EN 10213 are close but not the same either. For example, EN 1.4408 limits carbon to 0.07% and molybdenum to 2.0–2.5%.
When should you choose CF8?
Choose CF8 for general corrosion service where chlorides are low and the part will not be welded after heat treatment. Typical uses are valve and pump bodies for water, steam and many mild chemical duties. CF8 has no molybdenum addition, so it usually costs less than CF8M. It is weaker against pitting and crevice corrosion in chloride-bearing media.
When should you choose CF8M?
Choose CF8M when the medium contains chlorides, or when pitting and crevice corrosion are the main risk. Molybdenum improves resistance to both. Seawater, brackish water, many process chemicals and offshore duties usually call for CF8M or better. Our CF8M guide covers the grade in more detail.
CF8M does have limits. In warm, concentrated chlorides or strong acids, a duplex grade or a more highly alloyed austenitic grade may be needed. Give the medium, its concentration and its temperature when you ask for a recommendation.
When should you choose CF3M?
Choose CF3M when the casting will be welded and cannot be solution annealed afterwards. This includes welded assemblies, castings joined to pipework on site, and fabrication welds.
The reason is sensitisation. When a 0.08% carbon grade is heated during welding, chromium carbides can form at grain boundaries in the heat-affected zone. The metal next to them loses chromium and becomes open to intergranular corrosion. With carbon held to 0.03%, far less carbide can form, so CF3M keeps its corrosion resistance after welding. CF3M has the same molybdenum as CF8M, so it gives the same chloride resistance. If welding is not involved, CF8M is normally enough.
What about CF3 and CF8C?
Two related grades are worth knowing.
- CF3 is the low-carbon version of CF8, and the cast equivalent of 304L (EN 1.4309). It allows 0.03% carbon maximum, 17.0–21.0% chromium and 8.0–12.0% nickel. Use it where CF8 would suit but the casting will be welded.
- CF8C is CF8 stabilised with niobium, and the cast equivalent of 347. ASTM A351 requires niobium of at least eight times the carbon content, up to 1.00%. The niobium ties up carbon as niobium carbide, so less is left to form chromium carbides. It is mainly used for service at higher temperatures, where the stabilised structure resists sensitisation over long periods.
A quick way to decide
- Are chlorides present, or is pitting a concern? If yes, you need molybdenum: CF8M or CF3M.
- Will the casting be welded without a later solution anneal? If yes, you need low carbon: CF3 or CF3M.
- If neither applies, CF8 is usually the economical choice.
If the service is outside what these grades handle, see how to choose a casting material.
Casting these grades at H.J. MetalCraft
We cast CF8, CF8M, CF3 and CF3M to customer drawings, by sand casting up to 180 kg per piece and by investment casting from 10 g to 50 kg. Castings are solution annealed in-house and supplied raw or machined. See our stainless steel castings page and the standards and grades we work to, or send a drawing for a quote.
Equivalent grades are approximate. The grade and standard on your drawing govern.
Have a casting in mind? Send us the drawing.