Design
Steel casting tolerances (ISO 8062) and minimum wall thickness
ISO 8062-3 sets casting tolerances as grades (DCTG) and machining stock as allowance grades (RMAG). This guide explains both for steel sand and investment castings, and why steel needs thicker walls than iron or aluminium.
· Husein Jazakallah, Managing Director
Steel casting tolerances are normally specified to ISO 8062-3 as a dimensional casting tolerance grade (DCTG). Its Annex A puts steel sand castings at about DCTG 11 to 14 hand moulded and DCTG 8 to 12 machine moulded. Investment castings are tighter. Steel needs thicker walls than iron or aluminium; our stated minimum is 7 mm.
What is ISO 8062-3?
ISO 8062-3 is the international standard for general tolerances and machining allowances on castings of all metals. Its 2007 first edition replaced ISO 8062:1994, and the current edition is ISO 8062-3:2023.
The 1994 standard used single "CT" grades, which still appear on older drawings. The current standard uses three sets of grades:
- DCTG, dimensional casting tolerance grades, for linear dimensions;
- GCTG, geometrical casting tolerance grades, for form and orientation such as flatness and straightness;
- RMAG, required machining allowance grades, for the extra metal left on surfaces to be machined.
A complete drawing note gives the standard and its year, the DCTG, the GCTG if needed, and the RMAG.
What does a DCTG grade mean?
A DCTG grade sets the total permitted variation on an as-cast dimension. There are grades from DCTG 1, the finest, to DCTG 15. The 2023 edition renamed the coarsest grade, formerly DCTG 16, to DCTG 15wt. It applies to wall thickness only.
The tolerance depends on two things: the grade and the nominal size of the dimension. The table value is the total band. By default it is split evenly either side of the nominal size. For example, a dimension between 100 mm and 160 mm has a total tolerance of 3.6 mm at DCTG 10, or ±1.8 mm. At DCTG 12 the same dimension has a total tolerance of 7 mm.
For DCTG 1 to 15, wall thickness is toleranced one grade coarser than the general grade. A wall on a casting specified to DCTG 10 is checked at DCTG 11.
What DCTG can steel sand and investment castings achieve?
Annex A of ISO 8062-3 gives typical grades for each process and metal. It is informative guidance, not a requirement. For steel, published tables based on it give:
- Sand casting, hand moulded, long series production: DCTG 11 to 14.
- Sand casting, machine moulded and shell moulded, long series: DCTG 8 to 12.
- Single parts and short runs: coarser grades than long series.
- Investment casting: markedly tighter than sand casting.
The Steel Founders' Society of America (SFSA) publishes its own guidance, based on statistical studies of production steel castings. For long series it recommends CT 10 to 12 for most sand-cast parts and CT 5 to 7 for steel investment castings. For short series it moves each band about one grade coarser.
Treat these as starting points, and agree a grade with the foundry before fixing it on the drawing.
What drives casting tolerance?
Size. Longer dimensions vary more, because steel contracts as it cools. The patternmaker's contraction allowance for steel is around 2%, against about 1% or less for grey iron. Any variation in that contraction grows with length.
Parting line. Dimensions that cross the mould joint vary more than those inside one half of the mould. SFSA studies found the extra variation is significant in no-bake (chemically bonded) moulds. Put close-tolerance features on one side of the parting line where you can.
Cores. A feature formed between the mould and a core depends on where the core sits. That adds variation. Features formed by a single piece of tooling hold tighter tolerances.
Production quantity. Long runs let the foundry adjust the pattern after measuring first-off castings. Short runs do not, so they get coarser grades.
How should you handle draft?
Draft is the taper on faces perpendicular to the parting line that lets the pattern come out of the sand. Show it on the drawing, or state it in a note agreed with the foundry. The 2023 edition of ISO 8062-3 includes draft angle tables for each moulding method.
Draft is added before the tolerance is applied. Say whether a drafted dimension is measured at the top or bottom of the draft. Investment castings and cored features often need little or none.
What is required machining allowance (RMA)?
RMA is the extra metal left on a surface so that machining reaches clean, sound metal. It is not a tolerance, and it does not absorb dimensional errors. The casting tolerance applies on top of it.
RMA grades are letters. Unlike DCTG, the allowance is chosen from the largest overall dimension of the casting, not the size of the machined feature. A large casting therefore needs more stock on every machined face, even a small one.
Some faces need more than others. SFSA guidance recommends more stock on the top (cope) surface of a sand casting than on the bottom or sides. Place critical machined faces at the bottom of the mould (the drag) where possible.
We also supply castings fully machined; see machined components.
What is the minimum wall thickness for steel castings?
Published guides do not agree on one minimum wall for steel sand castings. It varies with grade, casting size and flow distance, so ask the foundry.
H.J. MetalCraft's stated minimum wall thickness is 7 mm. Our PED approval covers sand castings up to 180 kg and up to 65 mm thick.
Investment castings can usually have thinner walls than sand castings. The ceramic shell is preheated before pouring, so the metal loses heat more slowly and can fill thinner sections. For how the two processes compare, see sand casting vs investment casting.
Why does steel need thicker walls than iron or aluminium?
There are two reasons.
Fluidity. Steel is poured much hotter than iron or aluminium and starts to freeze quickly once it touches the mould. It does not flow as far in a thin section before it solidifies. Thin walls risk misruns and cold laps.
Shrinkage. Steel shrinks as it solidifies and contracts more as it cools. Grey iron partly offsets its shrinkage because graphite forms as it freezes. Steel has no such help, so every section must be fed with liquid metal from a feeder as it solidifies. Thin sections freeze early and cut off that feed to the metal beyond them.
How should you design a steel casting?
- Keep sections uniform. Sudden changes in thickness create hot spots that freeze last and can leave shrinkage porosity.
- Taper sections towards the feeders, so thick sections lie where the foundry can feed them.
- Use generous fillets. Sharp internal corners concentrate stress, form hot spots and can tear as the casting contracts.
- Avoid isolated heavy bosses and "+" junctions. Core bosses out and stagger ribs into "T" junctions.
- Talk to the foundry early. Small drawing changes can remove extra feeders, chills or rework.
State the inspection you need too. See NDT for steel castings.
Getting a quote
Put the ISO 8062-3 grades, critical dimensions and machined faces on the drawing. See how to write a casting RFQ, casting vs forging vs machining, duplex vs super duplex, standards and grades, our capabilities and investment casting. Then send your drawing through the quote form.
Have a casting in mind? Send us the drawing.
Request a quote